SAC305 Rosin Core Solder Wire
Industrial-Grade Lead-Free Solder Wire for SMT Assembly & PCB Repair
Product Specifications & Technical Data
|
Parameter |
Specification Details |
|
Alloy Composition |
Sn96.5 / Ag3.0 / Cu0.5 (Tin / Silver / Copper) |
|
Melting Point / Range |
217°C - 220°C (Eutectic behavior) |
|
Flux Type |
Rosin Core / RMA (Core ratio: 2.0% - 3.0%, customizable) |
|
Diameter Range |
0.3mm - 3.0mm (Customizable tolerances available) |
|
Surface Finish |
Bright silver metallic, oxide-free wire strand |
|
Compliance & Standards |
RoHS Compliant, IPC-J-STD-004 / 006, JIS Z 3282 |
|
Standard Packaging |
500g, 1kg plastic spools, vacuum-sealed in moisture-barrier bags with desiccant |
Core Performance Characteristics
Controlled Alloy Composition (Sn96.5/Ag3.0/Cu0.5): The precise 3.0% silver content increases shear strength and thermal fatigue resistance, while the 0.5% copper prevents excessive dissolution of copper pads during prolonged soldering. Batch-to-batch alloy purity is monitored via spectrometer analysis to eliminate wetting failures.
Rapid Wetting and Low Residue: The internal RMA-grade rosin core activates quickly at soldering temperatures (330°C - 380°C), breaking down surface oxides on copper traces and component leads. It leaves a minimal, non-corrosive, and high-insulation-resistance residue that meets electronic cleanliness standards.
Precision Wire Drawing and Spooling: Manufactured with strict diameter tolerances and uniform winding on plastic spools. This prevents feeding jams in automatic soldering stations and eliminates flux interruptions during continuous hand-soldering tasks.
Diameter Selection Guide
0.3mm - 0.8mm (Fine Gauge)
Engineered for fine-pitch SMT rework, micro-electronics repair, and dense PCB component installation.
1.0mm - 1.5mm (Medium Gauge)
Suited for general through-hole PCB assembly, electronic connectors, and multi-strand wire harness soldering.
2.0mm - 3.0mm (Heavy Gauge)
Applied in power electronics, busbars, heavy terminal connections, and industrial maintenance where high solder volume is required.
Manufacturing Quality Control
Raw Material Purity: Virgin metals (99.99% pure tin, silver, and copper) are melted under inert gas covers to eliminate dross and internal voids.
Extrusion & Drawing: Laser micrometers monitor wire diameter continuously during the cold drawing process to maintain strict dimensional uniformity.
Flux Core Injection: Automated synchronization ensures the rosin flux weight percentage remains stable (standard 2.2% or customized) along the entire length of the wire.
Global Customization & OEM/ODM Services
OEM Support Available: We offer flexible manufacturing solutions for global partners, including custom flux core percentages (e.g., 2.0% to 3.0%), customized spool weights (250g, 500g, 1kg), and private-label packaging tailored to your brand specifications.
FAQ
Q: What is SAC305 solder wire?
A: SAC305 solder wire is a lead-free solder alloy containing 96.5% tin, 3.0% silver, and 0.5% copper. It is one of the most commonly used lead-free solder alloys for electronics manufacturing.
Q: Why is SAC305 widely used in electronics?
A: SAC305 offers a good balance between solderability, mechanical strength, thermal reliability, and environmental compliance. It is suitable for many PCB assembly and electronic manufacturing applications.
Q: Is SAC305 solder wire RoHS compliant?
A: Yes, SAC305 is a lead-free solder alloy commonly used for RoHS-compliant electronic products. Customers should confirm specific regulatory requirements according to their market.
Q: What is the difference between SAC305 and Sn63/Pb37 solder wire?
A: The main difference is alloy composition. SAC305 is lead-free and melts at approximately 217°C, while Sn63/Pb37 contains lead and has a lower melting point of approximately 183°C. SAC305 is preferred where environmental regulations require lead-free materials.